Mannat Steel produces a diverse range of Stainless Steel Sheets and Plates. We carry stainless steel 304/304H sheets and plates, stainless steel 310s sheets and plates, stainless steel 316L sheets and plates, stainless steel 316H sheets and plates, stainless steel 904L sheets and plates, and much more. All of these goods are created from high-quality raw materials to provide our clients with a product that is proper Machinability and Durability with moderate strength and perfect finishing.
Stainless Steel 310s Sheets and Plates are commonly used in combustion chambers, lead pots, coal gasifiers, tube hangers for petroleum refining, refractory anchor bolts, retorts, food processing, cryogenic structures, and other applications. SS 310s have exceptional oxidation resistance and can withstand any hostile environment.
Pragati Metal fulfills our clients' orders in a safe and damage-free manner. We use a hefty thick fitting to pack SS 310s. We have a traditional professional team that has experience packing with numerous formalities. Pragati Metal is concerned with shipping; we deliver products on schedule and provide all details and documentation to our clients. We provide a variety of delivery options based on the needs of our customers.
Mannat Steel manufactures and exports high-quality 310s Stainless Steel Sheet, 310 SS Plates, and stainless steel 310 coils in thicknesses ranging from 0.3mm to 120mm, which have found extensive uses in a variety of sectors. We also deal in nickel and copper alloy, stainless and duplex steel, carbon and alloy steel, which are materials used in the design of stainless steel sheet, plates, and coils.
Standard | ASTM A240, ASME SA240 |
Thickness | 0.1mm to 12 mm Thk |
Sheet/Plate Size | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
Surface | 2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sandblast, Brush, etching. |
Finish | Hot rolled (HR), Cold rolled (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated), Galvanized etc. |
SS 310 Plate is a versatile material that is utilized in a variety of industries. Because of its capacity to resist oxidation and corrosion at high temperatures, it is frequently used in high-temperature services. Because of its high chromium and nickel alloy makeup, it can endure temperatures of up to 1050 degrees Celsius, making it excellent for a variety of industrial processes that need significant heat exposure. SS 310 Plate has good resistance to carburizing, nitriding, and oxidizing conditions, making it an excellent choice for applications such as heat exchangers and kilns. Aside from its heat resistance, SS 310 Plate also has significant strength and wear resistance capabilities, making it suitable for any application requiring high performance.
310S stainless steel plates are a chromium-nickel-based alloy that is commercially accessible. As a result, they have a one-of-a-kind composition that provides an optimal mix of strength, flexibility, and corrosion resistance. Furthermore, 310S stainless steel plates have a density of 8.0 g/cm3 or 0.289 lb/in3, making them relatively light in comparison to other metals with similar properties. Although they are not the lightest materials available, their low density allows them to be easily formed into complex shapes and sizes while still providing superior performance in the majority of applications.
STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
---|---|---|---|---|---|---|---|
SS 310 | 1.4841 | S31000 | SUS 310 | 310S24 | 20Ch25N20S2 | - | X15CrNi25-20 |
SS 310S | 1.4845 | S31008 | SUS 310S | 310S16 | 20Ch23N18 | - | X8CrNi25-21 |
Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
---|---|---|---|---|---|---|---|---|---|
SS 310 | 0.015 max | 2.0 max | 0.15 max | 0.020 max | 0.015 max | 24 – 26 | 0.10 max | 19 – 21 | 54.7 min |
SS 310S | 0.08 max | 2.0 max | 1.00 max | 0.045 max | 0.030 max | 24 – 26 | 0.75 max | 19 – 21 | 53.095 min |
Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
---|---|---|---|---|
7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |